Application Guide for the Furniture Workshop

Illustration of an orbital sander smoothing a timber board before finishing

This is the step by step method we use for finishing furniture, joinery and small timber components with Oslek LED Hardwax Oil. The whole process takes minutes rather than days, because each coat cures the moment the LED lamp passes over it. There is no overnight wait between coats and no curing room tied up for a week.

Not sure how much oil a job needs? Our guide to hardwax oil coverage and cost per square metre covers the maths.

What you'll need:

Oslek LED Hardwax Oil, a handheld LED curing lamp, roller and orbital buffer laid out ready for finishing furniture

Method:

  1. Prepare your surface to 120 grit to enable optimal oil penetration and adhesion.
  2. Apply the oil with a high-density roller and use an orbital buffer to burnish and buff the oil into the timber surface until even.
  3. Cure your first coat by holding your LED light approximately 2-3 cm above the surface and run it across the surface twice (back and forth).
  4. Once the first coat is cured, sand the surface to 180 grit.
  5. Repeat step 2 for the second coat. Please note that you will need significantly less oil on this coat.
  6. Repeat step 3 to cure.
  7. Once the second coat is cured, sand the surface to 320 grit or higher for your desired finish.
  8. Optional: Buff in any excess oil left on the buffer, roller or rag for a final coat. This is like a 'half' coat.
  9. Cure using your LED light.
  10. Your surface is ready to go!

Shop Now

Related reading

Try it on your own timber before you commit

The Sample Pouch has a mini LED torch, sachets of oil and instructions, so you can coat an offcut of your own stock and cure it in seconds. It is the quickest way to see whether this suits the work you do.

Order a Sample Pouch Read the full guide